PA66 408HS 美國(guó)杜邦公司 物性數(shù)據(jù) |
①原料描述部分
規(guī)格級(jí)別: | 注塑級(jí) | 外觀顏色: | --- |
用途概述: | --- | ||
備注說(shuō)明: | 特性:良好的熱穩(wěn)定性 |
②原料技術(shù)數(shù)據(jù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 |
|
數(shù)據(jù)單位 | |||||
基本性能 | 吸水率 | 24小時(shí)浸漬(23℃) | ASTM D-570 |
|
% | ||||
吸水率 | 飽和(23℃) | ASTM D-570 |
|
% | |||||
物理性能 | 比重 | --- | ASTM D-792 |
|
--- | ||||
機(jī)械性能 | 洛氏硬度M | --- | ASTM D-785 |
|
--- | ||||
洛氏硬度R | --- | ASTM D-785 |
|
--- | |||||
硬度計(jì)硬度 | --- | ASTM D-676 |
|
--- | |||||
拉伸強(qiáng)度 | 23℃ | ASTM D-638 |
|
MPa | |||||
屈服強(qiáng)度 | 23℃ | --- |
|
MPa | |||||
斷裂伸長(zhǎng)率 | 23℃ | ASTM D-638 |
|
% | |||||
屈服伸長(zhǎng)率 | --- | ASTM D-638 |
|
% | |||||
揉曲模量 | 23℃ | ASTM D-790 |
|
MPa | |||||
埃佐沖擊強(qiáng)度 | 23℃ | ASTM D-256 |
|
j/m | |||||
拉伸沖擊強(qiáng)度 | 長(zhǎng)試樣23℃ | ASTM D-1822 |
|
KJ/m2 | |||||
拉伸沖擊強(qiáng)度 | 短試樣23℃ | ASTM D-1822 |
|
KJ/m2 | |||||
電氣性能 | 體積電阻率 | --- | ASTM D-257 |
|
Ω.cm | ||||
介電常數(shù) | 100Hz(cps) | ASTM D-150 |
|
--- | |||||
介電常數(shù) | 103Hz(cps) | ASTM D-150 |
|
--- | |||||
介電常數(shù) | 106Hz(cps) | ASTM D-150 |
|
--- | |||||
耗散因數(shù) | 100Hz(cps) | ASTM D-150 |
|
--- | |||||
耗散因數(shù) | 103Hz(cps) | ASTM D-150 |
|
--- | |||||
耗散因數(shù) | 106Hz(cps) | ASTM D-150 |
|
--- | |||||
熱 性 能 | UL可燃性導(dǎo)級(jí) | --- | UL 94 |
|
--- | ||||
線性熱膨脹系數(shù) | --- | ASTM D-696 |
|
m/m/℃ | |||||
熔點(diǎn) | Fisher Johns法 | ASTM D-789 |
|
℃ | |||||
熔點(diǎn)結(jié)晶 | --- | ASTM D-2177 |
|
℃ | |||||
脆化溫度 | --- | ASTM D-746 |
|
℃ | |||||
荷重形變 | 13.8MPa,50℃ | ASTM D-621 |
|
% | |||||
熱畸變溫度 | 18×106Pa | ASTM D-648 |
|
℃ | |||||
熱畸變溫度 | (0.5)×106Pa | ASTM D-648 |
|
℃ | |||||
其它性能 | 需氧指數(shù) | --- | ASTM D-2863 |
|
% |