ABS 臺灣奇美 PA-756S注塑級
物性認證數(shù)據(jù)表
物性表 |
|||||
數(shù)據(jù)提供企業(yè)[ 東莞塑料超市 ] | 數(shù)據(jù)修正企業(yè)[ 暫無! ] |
|||||
性能項目 |
測試條件 |
測試方法 |
數(shù)值/描述 |
單位 |
|
機械性能 |
拉伸強度(引張強度) |
|
ASTM D638/ISO 527 |
385(5,470) |
kg/cm2(MPa)[Lb/in2] |
斷裂伸長率 |
|
ASTM D638/ISO 527 |
- |
% |
|
拉伸模量 |
|
ASTM D638/ISO 527 |
- |
kg/cm2(MPa)[Lb/in2] |
|
拉伸屈服伸長率(延伸率) |
|
ASTM D638/ISO 527 |
30 |
% |
|
拉伸斷裂伸長率(延伸率) |
|
ASTM D638/ISO 527 |
- |
% |
|
彎曲模量(彎曲彈性率) |
|
ASTM D790/ISO 178 |
24000(34000) |
kg/cm2(MPa)[Lb/in2] |
|
彎曲強度 |
|
ASTM D790/ISO 178 |
600(8,520) |
kg/cm2(MPa)[Lb/in2] |
|
洛氏硬度 |
|
ASTM D785 |
R-113 |
|
|
IZOD 缺口沖擊強度 |
1/4" 23℃ |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
|
1/4" -30℃ |
ASTM D256/ISO 179 |
17(3.1) |
kg·cm/cm(J/M)ft·lb/in |
||
1/8" 23℃ |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
||
1/8" -30℃ |
ASTM D256/ISO 179 |
20(3.7) |
kg·cm/cm(J/M)ft·lb/in |
||
Charpy沖擊強度 |
23℃ (缺口) |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
|
-30℃(缺口) |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
||
23℃(無缺口) |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
||
-30℃(無缺口) |
ASTM D256/ISO 179 |
- |
kg·cm/cm(J/M)ft·lb/in |
||
物性性能 |
比重(密度) |
|
ASTM D792/ISO 1183 |
1.05 |
|
成型收縮率 |
|
ASTM D955 |
- |
% |
|
熔融指數(shù)(流動系數(shù)) |
200℃/5kg |
ASTM D1238/ISO 1133 |
6.5 |
g/10min |
|
220℃/10kg |
ASTM D1238/ISO 1133 |
70 |
g/10min |
||
吸水率 23℃/24H |
|
ASTM D570/ISO 62 |
- |
% |
|
熱性能 |
熱變形溫度 |
退火 |
ASTM D648/ISO 75 |
99(210) |
℃(℉) |
未退火 |
ASTM D648/ISO 75 |
89(192) |
℃(℉) |
||
維卡軟化點 |
|
ASTM D1525/ISO R306 |
- |
℃(℉) |
|
熔點 |
|
- |
- |
℃(℉) |
|
燃燒性(率) |
|
UL94 |
1.6mmHB |
|
|
線性膨脹系數(shù) |
|
ASTM D696/ISO 11359 |
- |
mm/mm.℃ |
|
加工條件 |
干燥條件 |
|
|
80°C下烘料約2~3小時 |
|
加工溫度 |
射嘴 |
|
180~230°C |
℃ |
|
料筒前段 |
|
190~230 |
℃ |
||
料筒中段 |
|
190~230 |
℃ |
||
料筒后段 |
|
180~220 |
℃ |
||
熔體溫度 |
|
|
- |
℃ |
|
模具溫度 |
|
|
30~70°C |
℃ |
|
壓力 |
注塑壓力 |
|
- |
Mpa |
|
保壓壓力 |
|
- |
Mpa |
||
背壓 |
|
- |
Mpa |
||
螺桿轉速 |
|
|
- |
rpm |
|
其他 |
備注 |
在射出周期中勿將熱融膠長期停留在加熱管中 |
|||
顏色 |
- |
||||
特性 |
超高流動 中沖擊強度 |
||||
用途 |
性能相當于PA-757 / 可注射大面或薄肉成型品 / 磁碟片 |